- 類型:標(biāo)準(zhǔn)料
- 廠家(產(chǎn)地):日本旭化成
- 用途級(jí)別:注塑級(jí)
- 牌號(hào):SS9000
| 性能項(xiàng)目 | 測(cè)試條件 | 測(cè)試方法 | 數(shù)值/描述 | 單位 | |
| 機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 30 | kg/cm²(MPa)[Lb/in2] | |
| 斷裂伸長(zhǎng)率 | ASTM D638/ISO 527 | 20 | % | ||
| 拉伸模量 | ASTM D638/ISO 527 | kg/cm²(MPa)[Lb/in2] | |||
| 拉伸屈服伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
| 拉伸斷裂伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
| 彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 1482 | kg/cm²(MPa)[Lb/in2] | ||
| 彎曲強(qiáng)度 | ASTM D790/ISO 178 | 44 | kg/cm²(MPa)[Lb/in2] | ||
| IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg/cm²(MPa)[Lb/in2] | ||
| 1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
| -30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 23℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| -30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 硬度 A | ASTM D2240/ISO 868 | 75 | Shore A | ||
| 硬度 D | ASTM D2240/ISO 868 | Shore D | |||
| 物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.01 | ||
| 熔融指數(shù)(流動(dòng)系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | 8.0 | g/10min | |
| 220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
| 吸水率 23℃/24H | ASTM D570/ISO 62 | % | |||
| 光學(xué)性能 | 透光率 | ASTM D1003/ISO 13468 | % | ||
| 加工條件 | 干燥條件 | ||||
| 加工溫度 | 射嘴 | ℃ | |||
| 料筒前段 | ℃ | ||||
| 料筒中段 | ℃ | ||||
| 料筒后段 | ℃ | ||||
| 熔體溫度 | ℃ | ||||
| 模具溫度 | ℃ | ||||
| 壓力 | 注塑壓力 | Mpa | |||
| 保壓壓力 | Mpa | ||||
| 背壓 | Mpa | ||||
| 螺桿轉(zhuǎn)速 | rpm | ||||
| 其他 | 備注 | ||||
| 顏色 | |||||
| 特性 | |||||
| 用途 | |||||